Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C @Thickness 3.20 mm |
534 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C @Thickness 3.20 mm |
534 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific) LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI) Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI) Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Ensinger TECATOR™ TI 5031 Polyamide-imide (PAI), Bearing Grade TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
E-Polymers SEPAZ® V230B 30% Mineral Filled Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
E-Polymers SEPAZ® V240A 40% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | ASTM D648 |
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 279 °C | 534 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |