Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® 103 PC (Europe-Africa-Middle East) LEXAN 103 is a high viscosity U.V. stabilized multi purpose grade. LEXAN 103 is available in transparent, translucent and opaque colours. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | ASTM D648 |
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics Lexan® IR2840 PC (Europe-Africa-Middle East) IR 2840 resin is a medium-low flow (MFR = 6.5 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics Lexan® PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® VR2820 PC (Europe-Africa-Middle East) VR 2820 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | ASTM D648 |
Custom Resins Norpex® SE1 PPE (Polyphenylene Ether)
(discontinued **) High Performance FR. Properties for dry as molded samples.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | ASTM D648 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® FXD163R PC (Europe-Africa-Middle East) FXD163R is a Lexan PC Transparent grade in our VisualFX Portfolio. It is a light Diffusion effect, developed for today´s Aesthetic Differentiation Needs. Color package may effect properties, Ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | ISO 75 |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics PC0800 PC (Asia Pacific) PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | ASTM D648 |
Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled Conductive Carbon, Powder Modified with Flame Retardant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC721HFR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | ASTM D648 |
Stratasys® Polycarbonate A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 6.40 mm |
261 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C @Thickness 3.20 mm |
261 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | ASTM D648 |
Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | ASTM D648 |
Ashley Polymers Ashlene® RH190H2-B Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized with carbon black for outstanding weatherability.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD4412 PC Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |