Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® AG-30 PA66-GF30
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50
Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50
Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVL-5H nat PA*-GF50
Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70
Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70
Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40
Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following ..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50
Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50
Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac..
Deflection Temperature at 8.0 MPa 220 °C
428 °F
HDT/C; ISO 75-2
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..