Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 850 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer
Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer
Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp..
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Glow Wire Test 850 °C

@Thickness 1.60 mm
1560 °F

@Thickness 0.0630 in
Flammability Index; IEC 60695-2-12
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Glow Wire Test 850 °C

@Thickness 1.00 mm
1560 °F

@Thickness 0.0394 in
IEC 60695-2-12
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East)
LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of..
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® FC 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 850 °C

@Thickness 1.00 mm
1560 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Glow Wire Test 850 °C

@Thickness 1.60 mm
1560 °F

@Thickness 0.0630 in
IEC 60695-2-12
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features include Easy Molding, Mold Release.
Glow Wire Test 850 °C

@Thickness 1.60 mm
1560 °F

@Thickness 0.0630 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Glow Wire Test 850 °C

@Thickness 0.750 mm
1560 °F

@Thickness 0.0295 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
Glow Wire Test 850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
GWIT; IEC 60695-2-13
Covestro Makrolon® 2407 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng..
Glow Wire Test 850 °C

@Thickness 0.750 mm
1560 °F

@Thickness 0.0295 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 850 °C

@Thickness 1.00 mm
1560 °F

@Thickness 0.0394 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Glow Wire Test 850 °C

@Thickness 2.00 mm
1560 °F

@Thickness 0.0787 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 850 °C

@Thickness 1.00 mm
1560 °F

@Thickness 0.0394 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Glow Wire Test 850 °C

@Thickness 2.00 mm
1560 °F

@Thickness 0.0787 in
GWFI; IEC 60695
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black
Information provided by Eurotec®
Glow Wire Test 850 °C

@Thickness 2.20 mm
1560 °F

@Thickness 0.0866 in
GWFI; IEC 60695-2-12
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
Glow Wire Test 850 °C

@Thickness 1.00 mm
1560 °F

@Thickness 0.0394 in
GWIT
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® F 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Copyright © lookpolymers.com All Rights Reserved