Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -118 - -70.0 °C | -180 - -94.0 °F | Average value: -90.6 °C Grade Count:5 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Brittleness Temperature | -118 - -70.0 °C | -180 - -94.0 °F | Average value: -86.6 °C Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.6 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Brittleness Temperature | -100 - -70.0 °C | -148 - -94.0 °F | Average value: -79.3 °C Grade Count:8 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.4 °C Grade Count:14 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.6 °C Grade Count:9 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Brittleness Temperature | -71.0 - -70.0 °C | -95.8 - -94.0 °F | Average value: -70.2 °C Grade Count:5 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |