Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ HC 2155G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155G is a 55 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2155G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD795 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SVE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | |
Sibur 140-13 Compound 230/1 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | |
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 3800-75 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
TriStar TriSteel AC Metal Backed PTFE Bearing System Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 5565 General Purpose Molding FormulationNordel® IP 5565 |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 60/R1 Flexible PVC, Injection Molding for Footwear Anti-accident soles |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
Colorite Polymers Self Frosting™ 6811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 55/A Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 55 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D2137 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2350 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D-746 |
Axiall 18753 Wire & Cable Flexible PVC Non-lead stabilized, fungus resistant 105 C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D-746 |
Axiall 10750 Wire & Cable Flexible PVC General purpose 75C jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D-746 |
Axiall 19740 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | |
Colorite Polymers 6812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |