Polymer Property : Brittleness Temperature = -34.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable 1104L-xx61FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information p..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JC404HX Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R9788A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible XV3796 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 162 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS Compliant Uses: Armored Cable; Flexible JacketingForms: Pellets Agency Ratings: MIL C-915-C; MIL C-2194-D Additional Information: Shipboard Cables, armored Temperature R..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 3300-70 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Food Service Applications, Medical Applications, TubingAppearance-ClearForms-PelletsProcessing-Extrusio..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 3611-75 Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 585 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Features: General Purpose Uses: Tubing; Wire Jacketing Agency Ratings: UL 498; UL 62 Wire Types: SPT-1; SPT-2 Processing Method: ExtrusionForms: PelletsInformation Provided by ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 94-A0055A-80 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 1700-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsAppearance- Natural Color, OpaqueInformation provided by Teknor Apex Company
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Teknor Apex APEX® 2070-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi..
Brittleness Temperature -37.0 °C
-34.6 °F
Sylvin Technologies 5100 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -37.0 °C
-34.6 °F
Cold Flex; ISO 458/2
Fainplast Compounds CTS 55/1 Flexible PVC, Extrusion Modified with Rubber
Profiles high elasticity
Brittleness Temperature -37.0 °C
-34.6 °F
Cold Flex; ISO 458/2
Fainplast Compounds HGKA 81 Flexible PVC, Sheathing for High Temperatures Lead Free
Sheath high flexibility
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746A
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 31508/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. PVDF 31508/0003 also has a very low brittleness temperature, for..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746A
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A ..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746A
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly..
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D-746
Axiall 14700 Wire & Cable Flexible PVC
Clear, flexible PVC compound recommended for SPT applications. Maximum service temperature rating of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -37.0 °C
-34.6 °F
Sylvin Technologies 6150-80 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746A
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride  (discontinued **)
Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M..
Brittleness Temperature -37.0 °C
-34.6 °F
Cold Flex; ISO 458/2
Fainplast Compounds PM 65/R Flexible PVC, Lead Free
Extrusion modified with rubber
Brittleness Temperature -37.0 °C
-34.6 °F
ASTM D746
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..