| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable JC404HX Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 66 | 66 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 13.1 MPa | 1900 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 390 % | 390 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -37.0 °C | -34.6 °F | ASTM D746 |
| Flammability, UL94 | V-0 <br>@Thickness 3.00 mm |
V-0 <br>@Thickness 0.118 in |
BK; UL 94 |
| Oxygen Index | 27 % <br>@Thickness 1.91 mm |
27 % <br>@Thickness 0.0752 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 155 - 165 °C | 311 - 329 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | CSA C-22.2 No. 6 VO (LS86302-2) | |
| UL QMFZ2 | ||
| Features | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 85% | 121°C, 1.91 mm; 336 hr, UL Standard |
| Retention of Tensile Strength | 99% | 121°C, 1.91 mm; 336 hr, UL Standard |
| Uses | Wire & Cable Applications |