Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat
(discontinued ** High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen.. |
|||
Brittleness Temperature | -118 °C | -180 °F | ASTM D 746 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Brittleness Temperature | -118 - -70.0 °C | -180 - -94.0 °F | Average value: -90.6 °C Grade Count:5 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Brittleness Temperature | -118 - -75.0 °C | -180 - -103 °F | Average value: -94.3 °C Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Brittleness Temperature | -118 - 82.2 °C | -180 - 180 °F | Average value: -82.3 °C Grade Count:137 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Brittleness Temperature | -118 - -75.0 °C | -180 - -103 °F | Average value: -87.7 °C Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Brittleness Temperature | -118 - -70.0 °C | -180 - -94.0 °F | Average value: -86.6 °C Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D 746 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Ineos TC46-25 HDPE TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D 746 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Brittleness Temperature | -118 °C | -180 °F | ASTM D746 |
Total HDPE XT10 N High Density Polyethylene - Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Formosa Plastics Formolene® E900 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E900 is a high molecular weight high density polyethylene (HMW-HDPE) resin des.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Formosa Plastics Formolene® HB5502A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5502A is designed for applications requiring excellent stiffness and stress crack resistance properties. It.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Formosa Plastics Formolene® HB6007 Blow Molding HDPE HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excell.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: L.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce.. |
|||
Brittleness Temperature | -118 °C | -180 °F | ASTM D746 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Diamond Polymers NPP50-0355 High Density Polyethylene Blow Molding/Extrusion Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® HHM 4903 High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerCustomer Benefits: A high performance copolymer that can measure up to the most demanding application. Specifically formulated to provide toughness and durabil.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Brittleness Temperature | -118 - -59.0 °C | -180 - -74.2 °F | Average value: -81.5 °C Grade Count:55 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Amco PRIMATOP HDPE 003952 Phillips Process Hexene Copolymer HDPE 003952 features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco produ.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Amco PRIMATOP HDPE 003955P Phillips Process Hexene Copolymer HDPE 003955P features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco prod.. |
|||
Brittleness Temperature | <= -118 °C | <= -180 °F | ASTM D746 |
Formosa Plastics Formolene® HB5502B2 Blow Molding HDPE Hexene CopolymerApplications: Pharmaceutical Packaging; Personal Care Products;
Bleach and Detergents Industrial; and Chemicals & PartsFormolene® HB5502B2 is designed for applications requiring ex.. |
|||
Brittleness Temperature | -118 °C | -180 °F | ASTM D 746 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |