Material Notes:
TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-25 balances stiffness, ESCR and molecular weight to provide required toughness and crush strength without compromising processability.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 96 hour
>= 96 hour
Condition B, F20, 100% Igepal; ASTM D1693
>= 192 hour
>= 192 hour
Condition C, F0, 100% Igepal; ASTM D1693
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
ASTM D3895 modified (excludes copper mesh), 200°C
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Yield 23.4 MPa
3390 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 800 %
>= 800 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 0.897 GPa
130 ksi
2% Secant-Method 1; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
ASTM D648
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Descriptive Properties Value Comments
Process Extrusion
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved