Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers GTPO8280 NATURAL PVC Application: EPDM Based flexible polyolefin compound.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 65 A Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 - -16.0 °C | -67.0 - 3.20 °F | Average value: -34.1 °C Grade Count:16 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | ASTM D746 |
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | MTM 17238 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 4510/R Flexible PVC, Injection Molding for Footwear Vamp Boots with Rubber |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 46/T Flexible PVC, Injection Molding for Footwear Vamp boots |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | XT<sub>b</sub>; ASTM D746 |
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | XT<sub>b</sub>; ASTM D746 |
Colorite Polymers Elastichem 5511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1532WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 45/1 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
AlphaGary Garaflex™ E 50-10 B Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable90°C rated non-migrating jacket compound for Mil C 17G |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers 6014 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |