Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.750 mm
239 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT  (Unverified Data**)
Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
UL RTI, Mechanical with Impact 115 °C

@Thickness 6.00 mm
239 °F

@Thickness 0.236 in
UL 746B
DuPont Performance Polymers Crastin® S600F10 BK851 PBT  (Unverified Data**)
Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® S600F10 BK851 PBT  (Unverified Data**)
Crastin® S600F10 BK851 is an unreinforced, lubricated, medium high viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® S600F40 BK851 PBT  (Unverified Data**)
Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness 6.00 mm
239 °F

@Thickness 0.236 in
UL 746B
DuPont Performance Polymers Crastin® SK601 BK851 PBT  (Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® SK602 BK851 PBT  (Unverified Data**)
Crastin® SK602 BK851 is a 15% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 115 °C

@Thickness >=1.60 mm
239 °F

@Thickness >=0.0630 in
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=1.50 mm
239 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=3.00 mm
239 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=1.50 mm
239 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1301EP30 Polycarbonate Resin
Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=1.50 mm
239 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1301V-10 Polycarbonate Resin
Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.60 - 1.70 mm
239 °F

@Thickness 0.0630 - 0.0669 in
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=3.00 mm
239 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin
Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 115 °C

@Thickness >=1.70 mm
239 °F

@Thickness >=0.0669 in
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0591 in
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0591 in
NC, BK
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.57 mm
239 °F

@Thickness 0.0618 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 3.17 mm
239 °F

@Thickness 0.125 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.57 mm
239 °F

@Thickness 0.0618 in
UL 746
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.57 mm
239 °F

@Thickness 0.0618 in
UL 746
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 3.17 mm
239 °F

@Thickness 0.125 in
UL 746
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.780 mm
239 °F

@Thickness 0.0307 in
UL 746
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 1.57 mm
239 °F

@Thickness 0.0618 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical with Impact 115 °C

@Thickness 0.750 mm
239 °F

@Thickness 0.0295 in
DAM; UL 746B
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Copyright © lookpolymers.com All Rights Reserved