Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 130 °C @Thickness 0.800 mm |
266 °F @Thickness 0.0315 in |
UL 746 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 1.60 mm |
266 °F @Thickness 0.0630 in |
UL 746 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 0.851 mm |
266 °F @Thickness 0.0335 in |
UL 746 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.30 mm |
266 °F @Thickness >=0.130 in |
|
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=0.710 mm |
266 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.30 mm |
266 °F @Thickness >=0.130 in |
|
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=0.710 mm |
266 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=0.320 mm |
266 °F @Thickness >=0.0126 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 24 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 0.710 mm |
266 °F @Thickness 0.0280 in |
UL746B |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G8F 23 R Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |