Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 5.99 mm |
185 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 5.99 mm |
185 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness >=2.00 mm |
185 °F @Thickness >=0.0787 in |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |