Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.851 mm
284 °F

@Thickness 0.0335 in
UL 746
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Mechanical with Impact 140 °C

@Thickness 1.60 mm
284 °F

@Thickness 0.0630 in
UL 746
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Mechanical with Impact 140 °C

@Thickness 2.30 mm
284 °F

@Thickness 0.0906 in
UL 746
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Mechanical with Impact 140 °C

@Thickness 3.00 mm
284 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 140 °C

@Thickness 3.00 mm
284 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FB PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FB PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FC PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FC PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=3.00 mm
284 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2306FC PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FI PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FI PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=3.00 mm
284 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2306FI PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FS PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FS PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=3.00 mm
284 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2306FS PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FG PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FG PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=3.00 mm
284 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2306FG PBT+GF30%
Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical with Impact 140 °C

@Thickness >=0.710 mm
284 °F

@Thickness >=0.0280 in
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=1.50 mm
284 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
UL RTI, Mechanical with Impact 140 °C

@Thickness >=3.00 mm
284 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
UL RTI, Mechanical with Impact 140 °C

@Time 7.20e+7 sec
284 °F

@Time 20000 hour
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R..
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Rynite® 545 BK504 PET  (Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..
UL RTI, Mechanical with Impact 140 °C

@Thickness 3.00 mm
284 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Rynite® 545 BK504 PET  (Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.810 mm
284 °F

@Thickness 0.0319 in
UL 746B
DuPont Performance Polymers Rynite® 545 BK504 PET  (Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..