Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® GW520CS NC010 PET
(Unverified Data**) Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 140 °C @Thickness >=3.30 mm |
284 °F @Thickness >=0.130 in |
|
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 270 PBT-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.800 mm |
284 °F @Thickness 0.0315 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.60 mm |
284 °F @Thickness 0.0630 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
UL RTI, Electrical | 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |