Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East) LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 923X PC Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL746B |
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL746B |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL746B |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific) 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746 |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746 |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
|
Covestro Makrolon® 9125 Polycarbonate Medium viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |