Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 155 °C @Thickness 0.810 mm |
311 °F @Thickness 0.0319 in |
UL 746B |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 155 °C | 311 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Mechanical with Impact | 155 °C | 311 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Mechanical with Impact | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
BK |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |