Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 940ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 945A PC (Asia Pacific) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 945AU PC (Asia Pacific) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL746B |
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL746B |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL746 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.47 mm |
248 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® G-3310M Isotropic, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 10 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 953A PC (Europe-Africa-Middle East) LEXAN 953A is a high viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® 943 PC (Europe-Africa-Middle East) LEXAN 943 is a medium viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Asia Pacific) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |