Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical with Impact = 155 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 155 °C

@Thickness 0.810 mm
311 °F

@Thickness 0.0319 in
UL 746B
DuPont Performance Polymers Rynite® RE19051 BK507 PET  (Unverified Data**)
Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 155 °C
311 °F
UL 746B
SABIC Innovative Plastics ULTEM CRS5011 PEI
Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing.
UL RTI, Mechanical with Impact 155 °C
311 °F
UL 746B
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific)
Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing.
UL RTI, Mechanical with Impact 155 °C

@Thickness 1.50 mm
311 °F

@Thickness 0.0591 in
BK
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..
Copyright © lookpolymers.com All Rights Reserved