Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 75.0 - 130 °C | 167 - 266 °F | Average value: 112 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
UL RTI, Electrical | 50.0 - 130 °C | 122 - 266 °F | Average value: 95.0 °C Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
UL RTI, Electrical | 125 - 130 °C | 257 - 266 °F | Average value: 126 °C Grade Count:4 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
UL RTI, Electrical | 80.0 - 130 °C | 176 - 266 °F | Average value: 102 °C Grade Count:13 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
UL RTI, Electrical | 80.0 - 130 °C | 176 - 266 °F | Average value: 109 °C Grade Count:13 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
UL RTI, Electrical | 65.0 - 130 °C | 149 - 266 °F | Average value: 89.2 °C Grade Count:9 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
UL RTI, Electrical | 65.0 - 130 °C | 149 - 266 °F | Average value: 122 °C Grade Count:3 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
UL RTI, Electrical | 50.0 - 130 °C | 122 - 266 °F | Average value: 119 °C Grade Count:3 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |