Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 0.020" (0.508 mm) Flexible Heater Silicone with Fiberglass Substrate (51576R020) Cured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.009 in. (0.2 mm); 0.003 i.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579A028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 30570R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 51571R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene Appearance: Black silicone gum on fiberglass clothThis da.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per card E54153 |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E54153 |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44576XB015 0.015" (0.381 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum and rubber on fiberglass clothThis data represents typical values for the production ma.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon CP-427R Silicone Rubber bulk compound |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E54153 |
Arlon R34688XA030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured/Cured LayersThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 48271R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater .. |