Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 246 - 280 °C
475 - 536 °F
Average value: 262 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Deflection Temperature at 0.46 MPa (66 psi) 200 - 280 °C
392 - 536 °F
Average value: 264 °C Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Deflection Temperature at 0.46 MPa (66 psi) 266 - 280 °C
510 - 536 °F
Average value: 270 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Deflection Temperature at 0.46 MPa (66 psi) 260 - 280 °C
500 - 536 °F
Average value: 274 °C Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Deflection Temperature at 0.46 MPa (66 psi) 260 - 280 °C
500 - 536 °F
Average value: 267 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Deflection Temperature at 0.46 MPa (66 psi) 260 - 280 °C
500 - 536 °F
Average value: 268 °C Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Deflection Temperature at 0.46 MPa (66 psi) 238 - 280 °C
460 - 536 °F
Average value: 263 °C Grade Count:9
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..