Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 108 - 215 °C | 226 - 419 °F | Average value: 170 °C Grade Count:31 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | Average value: 213 °C Grade Count:3 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 215 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 220 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 220 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 220 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 230 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 230 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 220 12HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 215 °C | 410 - 419 °F | ASTM D1525, HDT Method B |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 - 215 °C | 221 - 419 °F | Average value: 166 °C Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 - 215 °C | 230 - 419 °F | Average value: 176 °C Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 - 215 °C | 290 - 419 °F | Average value: 166 °C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |