Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 100 - 150 °C | 212 - 302 °F | Average value: 123 °C Grade Count:7 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 145 - 150 °C | 293 - 302 °F | ASTM D1525, HDT Method B |
Loxim 120 01V0 Polycarbonate, 20% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 70.0 - 150 °C | 158 - 302 °F | Average value: 140 °C Grade Count:20 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 - 150 °C | 201 - 302 °F | Average value: 128 °C Grade Count:140 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |