Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 106 °C
176 - 223 °F
Average value: 94.3 °C Grade Count:52
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Deflection Temperature at 0.46 MPa (66 psi) 42.0 - 106 °C
108 - 223 °F
Average value: 72.4 °C Grade Count:25
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Deflection Temperature at 0.46 MPa (66 psi) 87.8 - 106 °C
190 - 223 °F
Average value: 94.4 °C Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Deflection Temperature at 0.46 MPa (66 psi) 91.0 - 106 °C
196 - 223 °F
Average value: 100 °C Grade Count:7
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..