Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF17 IM2 L 17% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 17% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedInformatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 CM25 HS BK 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M20 IM BK 20% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat S.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 HS Up BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat Sta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF33 TL10 HS 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF33 TL10 HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF8 IM3 BK 8% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 03004 GF20 Carbon/20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 485 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 03005 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |