Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 - 235 °C | 380 - 455 °F | Average value: 216 °C Grade Count:3 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CM30 HS BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/12 01430 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | ASTM D648 |
Chase Plastics CP Pryme® N100MD2 (COND, 50% RH) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | ASTM D648 |
Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 380 °F | ASTM D648 |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |