Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Ravago Manufacturing Americas Hylex® P10017FRMA Polycarbonate Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Global MPP-140-C 40% Mica Reinforced Polypropylene Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE 0226 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE MM40 40% Mica Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mica Filler, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: LubricatedAppearance: BlackInformation provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® TPX-PA6-95002 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | annealed; ASTM D648 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | annealed; ASTM D648 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Unannealed; ASTM D648 |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Asahi Kasei Thermylene® P1-10FG-8100 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Aaron Industries AAROPRENE® GFPP 2040 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ MP-10GF/10T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 143 °C | 290 °F | ASTM D648 |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |