Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 195 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black
Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C

@Thickness 3.18 mm
195 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black
Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Ineos H01H-00 Polypropylene Homopolymer
This is a low flow rate homopolymer designed for extrusion or injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applic..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible Polypropylene Random Copolymer
A biocompatible approx. 10 melt injection molding grade of Polypropylene random copolymer for healthcare applications.All information provided by LTL Color Compounders, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer
A biocompatible( approx. 10 melt Polypropylene random copolymer for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer
A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Ineos R12C-01 Polypropylene Random Copolymer
Grade R12C-01 is a high clarity, antistatic polypropylene copolymer for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Food and Drug Admini..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Spartech PP7110 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM Test
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
unannealed; ASTM D648
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 9035 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Washington Penn Medium Impact Copolymer 20% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Americas Styrenics STYRON A-TECH® 1170 High Impact Polystyrene
Product CharacteristicsGood impact resistanceConsistent colorabilityEasy processingFood Contact CompliantUL Classification 94HBTypical ApplicationsExtruded SheetSmall AppliancesRefrigeration Accesso..
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Aaron Industries AVPP C 200-2 MELT 30 Clarified Virgin Polypropylene
A natural polypropylene copolymer resin specifically designed for injection molding applications - containing clarifiers.
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Asahi Kasei Thermofil P-10CC-1417 10% Calcium Carbonate Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Copyright © lookpolymers.com All Rights Reserved