Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.4 °C | 170 °F | Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.9 °C | 170 °F | 0.125 in bar; ASTM D648 |
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.9 °C | 170 °F | ASTM D618 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.5 °C | 170 °F | Unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Ineos N20G-00 Polypropylene Impact Copolymer Grade N20G-00 is a high melt flow rate “super-high†impact copolymer polypropylene for injection molding applications. It offers very high impact resistance and good stiffness. This materi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Ecomass® 3620BX18 5% Borated Polyethylene (HDPE) 5% Borated Polyethylene (HDPE), Product Form - Pellets, No Pre-Drying RequiredProcessing Method: Injection Molding, Compression MoldingNeutron Shielding ApplicationsInformation provided by Technica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE HD 300-2 Black BM High Density Polyethylene, Blow Molding AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, HDPE Black, Blow Molding GradeFeatures: A high density Polyethylene compound, pre-colored black, specifically designed for all blow molding.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE HD 300-2 Black Crate High Density Polyethylene Compounded Resin, Crate Grade AAROLENE® ARPE 300 Series Polyethylene Compounded Resin HDPE, Black Crate GradeFeatures: A high density Polyethylene compound, pre-colored black, specifically designed for all crate applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.7 °C | 170 °F | ASTM D648 |
Ineos H48-500-199 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for roll-out cart applications. This material meets the Food and Drug Administration req.. |