Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 57.2 °C | 135 °F | ASTM D648 |
RheTech Products E206-01 Linear Low Density Polyethylene, Black Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 - 92.0 °C | 135 - 198 °F | Average value: 79.5 °C Grade Count:4 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 - 92.0 °C | 135 - 198 °F | Average value: 74.1 °C Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
SPS Guang Zhou POPTREEâ„¢ 6001 Flame-retarded Polyethylene Characteristic: Low density, superior melt flow index, high notched impact strengthApplications: X'mas decorative productInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | |
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | Unannealed; ASTM Data |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ISO 75-1/-2 |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 - 99.0 °C | 135 - 210 °F | Average value: 73.1 °C Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 °C | 135 °F | ASTM D648 |
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formula.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.0 - 93.0 °C | 135 - 199 °F | Average value: 78.3 °C Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 57.2 °C | 135 °F | Annealed; ASTM D648 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |