Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 246 - 280 °C | 475 - 536 °F | Average value: 262 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 - 280 °C | 392 - 536 °F | Average value: 264 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 266 - 280 °C | 510 - 536 °F | Average value: 270 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 260 - 280 °C | 500 - 536 °F | Average value: 274 °C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 260 - 280 °C | 500 - 536 °F | Average value: 267 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 260 - 280 °C | 500 - 536 °F | Average value: 268 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 238 - 280 °C | 460 - 536 °F | Average value: 263 °C Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |