Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 260 °C | 410 - 500 °F | Average value: 219 °C Grade Count:15 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 190 - 260 °C | 374 - 500 °F | Average value: 230 °C Grade Count:56 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 - 260 °C | 428 - 500 °F | Average value: 255 °C Grade Count:20 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 260 °C | 410 - 500 °F | Average value: 247 °C Grade Count:13 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 - 260 °C | 464 - 500 °F | Average value: 253 °C Grade Count:15 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 - 260 °C | 464 - 500 °F | Average value: 257 °C Grade Count:14 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 124 - 260 °C | 255 - 500 °F | Average value: 231 °C Grade Count:54 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 188 - 260 °C | 370 - 500 °F | Average value: 234 °C Grade Count:10 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 - 260 °C | 185 - 500 °F | Average value: 192 °C Grade Count:11 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 155 - 260 °C | 311 - 500 °F | Average value: 223 °C Grade Count:50 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 - 260 °C | 464 - 500 °F | Average value: 255 °C Grade Count:6 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 - 260 °C | 230 - 500 °F | Average value: 198 °C Grade Count:17 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |