Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 144 - 221 °C
292 - 430 °F
Average value: 205 °C Grade Count:19
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® 6MPY Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® 6PA-Blue Nylon 6
NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® 6PA-MoS2 Nylon 6
NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade
NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
400 - 430 °F
ASTM D648
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® Nyloil® Lubricated Nylon
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6
Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat..
Deflection Temperature at 0.46 MPa (66 psi) 160 - 221 °C
320 - 430 °F
Average value: 203 °C Grade Count:30
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Deflection Temperature at 0.46 MPa (66 psi) 213 - 221 °C
415 - 430 °F
Average value: 218 °C Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved