Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 149 °C
185 - 300 °F
Average value: 112 °C Grade Count:18
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 0.46 MPa (66 psi) 135 - 149 °C
275 - 300 °F
Average value: 144 °C Grade Count:8
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 0.46 MPa (66 psi) 132 - 149 °C
270 - 300 °F
ASTM D648
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Deflection Temperature at 0.46 MPa (66 psi) 136 - 149 °C
277 - 300 °F
Average value: 145 °C Grade Count:46
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Deflection Temperature at 0.46 MPa (66 psi) 74.0 - 149 °C
165 - 300 °F
Average value: 99.8 °C Grade Count:12
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Deflection Temperature at 0.46 MPa (66 psi) 121 - 149 °C
250 - 300 °F
Average value: 141 °C Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Deflection Temperature at 0.46 MPa (66 psi) 97.2 - 149 °C
207 - 300 °F
Average value: 122 °C Grade Count:21
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..
Deflection Temperature at 0.46 MPa (66 psi) 101 - 149 °C
214 - 300 °F
Average value: 129 °C Grade Count:24
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..