Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 - 98.9 °C | 180 - 210 °F | |
Fibre Glast 182 White Gel Coat #182 White Gel Coat is a highly durable ISO gel coat and is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | unannealed; ASTM D648 |
I. Stern 2335C Prime Clarified Random Copolymer Polypropylene Features:High flow characteristicsFDASee-through and contact clarityFood contact acceptableApplicationsContainersBottlesStorage boxesToysInformation provided by I. Stern & Co. Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | annealed; ASTM D648 |
KYDEX® 6200 LTR Thermoforming Sheet for Mass Transit Applications Features:Specifically designed for mass transit industriesCompliant with SMP800CMeets flamespread and smoke density requirements for mass transitExcellent formability and fabrication qualityGood def.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifaxâ„¢ CB251 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB251 medium melt flow, 1,200 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact resis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Westlake Plastics TPX® Polymethylpentene TPX is a lightweight, high temperature polyolefin with exceptional acoustical and electrical properties. TPX has low moisture absorption and excellent chemical resistance. It is often used for app.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
CPC - Vycom PLAYBOARD™ HDPE Sheet for Modular Playground Systems Playboard Modular Playground Systems consists of 2-color PolyCarve™ co-extruded sheet and Grip X™ slip resistant sheet materials.FEATURES AND BENEFITS Weather resistant- Playboard is UV stabilized.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
CPC - Vycom SEABOARD™ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | annealed; ASTM D-648 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin HDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPE LD 300-1 LDPE Black Low Density Polyethylene AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, LDPE BlackFeatures: A compounded LDPE, black, low melt resin specifically designed for all profile extrusion applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aclo Accucomp Polypropylene HPO309L Homopolymer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ASTM D648 |
Aclo Accucomp Polystyrene HS0600L High Impact |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C | 180 °F | ISO 75-2/B |
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac.. |