Material Notes:
AAROLENE® ARPE 300 Series Polyethylene Compounded Resin HDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified.
Physical Properties Metric English Comments
Specific Gravity 0.950 - 0.962 g/cc
0.950 - 0.962 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 0.30 - 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 - 50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 28.3 MPa
4100 psi
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648