Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Network Polymers MS 130HF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 - 145 °C | 169 - 293 °F | Average value: 117 °C Grade Count:35 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | |
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade Easy-to-process blow molding grade for stackable canisters (up to 60 l), used for packing surface-active liquids, laundry and dishwashing detergents, disinfectants, drums (up to 220 l) for various s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® H6030 High Density Polyethylene ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5008 High Density Polyethylene ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® M6138 High Density Polyethylene ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 12.7 mm |
169 °F @Thickness 0.500 in |
ASTM D648 |
LG Chemical LUTENE-H BE0350 HDPE Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Ineos T50-2000 HDPE Ineos T50-2000 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It is c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® L5876 High Density Polyethylene, Blow Molding Grade ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 3.17 mm |
169 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C @Thickness 3.17 mm |
169 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 109 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 - 100 °C | 169 - 212 °F | Average value: 85.1 °C Grade Count:9 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
LyondellBasell Alathon® 9301 High Density Polyethylene ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F.. |