Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648-95 |
Multibase Multi-Flex® TPO DEFA 1037 Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 345-009 is a low density homopolymer resin designed for blow molding applications. Excellent clarity combined with strength and high stiffness makes NA 345-009 an ideal ch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
LyondellBasell Purell® PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3020 D is a low density polyethylene with high rigidity, good opticals and good chemical resistance. It is delivered in pellet form. Target markets are small blow molding including packagi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
UBE P7115U Electronic Grade Nylon Copolymer Powder Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C @Thickness 3.17 mm |
115 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 - 47.0 °C | 115 - 117 °F | UV Postcure; ASTM D648-98c |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | |
Covestro Texin® 270 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | |
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM-D648 |
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM-D648 |
Braskem ML2400N LLDPE Injection Molding Polyethylene The resin ML2400N is a linear low-density polyethylene, 1-butene based, with good flexibility and low warpage. It does not contain a slip agent. It does have narrow molecular weight distribution. Th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 - 187 °C | 115 - 369 °F | Average value: 91.5 °C Grade Count:42 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 46.0 °C | 115 °F | ASTM D648 |
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |