Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 0% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 20% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 20% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 40% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 40% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes 214® alloy, 30% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 25.0 - 900 °C |
9.78 µin/in-°F @Temperature 77.0 - 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 21.0 - 815 °C |
9.78 µin/in-°F @Temperature 69.8 - 1500 °F |
Mean |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 75.0 °C |
9.78 µin/in-°F @Temperature 167 °F |
|
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 500 °C |
9.78 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum 309Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 800 °C |
9.78 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367) The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 300 °C |
9.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 538 °C |
9.78 µin/in-°F @Temperature 68.0 - 1000 °F |
|
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286 Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at .. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 800 °C |
9.78 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 800 °C |
9.78 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 800 °C |
9.78 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
CTE, linear | 17.6 µm/m-°C @Temperature 20.0 - 800 °C |
9.78 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |