Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.6 µm/m-°C @Temperature 0.000 - 500 °C |
7.00 µin/in-°F @Temperature 32.0 - 932 °F |
|
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 20.0 - 200 °C |
7.00 µin/in-°F @Temperature 68.0 - 392 °F |
|
International Mold Steel NAK55 Precipitation Hardened Mold Steel Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.0 - 427 °C |
7.00 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe LSSâ„¢ S5 Shock-Resisting Tool Steel (ASTM S5) TLS S5 Shock-Resisting tool steel is a silicon-manganese tool steel which exhibits the highest impact toughness among all of the "S" type steels. The high toughness and the ability to be hardened to.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 200 °C |
7.00 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 300 °C |
7.00 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 20.0 - 316 °C |
7.00 µin/in-°F @Temperature 68.0 - 601 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 399 °C |
7.00 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 399 °C |
7.00 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 93.3 °C |
7.00 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 300 °C |
7.00 µin/in-°F @Temperature 70.0 - 572 °F |
|
Crucible Steel KAPSTAR® Mold Steel Kapstar is a high hard, precipitation hardening mold steel suitable for production of machined or EDM’d plastic mold, rubber mold, and zinc die casting die components. Kapstar is supplied at about .. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 427 °C |
7.00 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 204 °C |
7.00 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel MAXEL® 3-1/2 (Brake Die) Free-Machining Alloy Steel, AISI 4150 S MAXEL 3-1/2 free-machining alloy steel provides a good combination of heat treated properties and machinability. This alloy steel is manufactured under close quality control to an ASTM grain size of.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 20.0 - 205 °C |
7.00 µin/in-°F @Temperature 68.0 - 401 °F |
|
Crucible Steel S7 (AISI S7) Tool Steel Crucible S7 is a shock resisting tool steel with excellent toughness and high strength, along with low to medium wear resistance. It has been widely used for many years to make chisels and punches w.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 399 °C |
7.00 µin/in-°F @Temperature 750 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 427 - 788 °C |
7.00 µin/in-°F @Temperature 801 - 1450 °F |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 25.0 - 100 °C |
7.00 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.1 - 399 °C |
7.00 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.0 - 204 °C |
7.00 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 24.0 - 316 °C |
7.00 µin/in-°F @Temperature 75.2 - 601 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
CTE, linear | 12.6 µm/m-°C @Temperature 21.0 - 200 °C |
7.00 µin/in-°F @Temperature 69.8 - 392 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |