Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.9 µm/m-°C @Temperature 30.0 - 100 °C |
6.60 µin/in-°F @Temperature 86.0 - 212 °F |
|
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type) PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 204 °C |
6.60 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
H1150 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
H1150 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
H1150 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 0.000 - 649 °C |
6.60 µin/in-°F @Temperature 32.0 - 1200 °F |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 788 °C |
6.60 µin/in-°F @Temperature 68.0 - 1450 °F |
|
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 93.3 °C |
6.60 µin/in-°F @Temperature 68.0 - 200 °F |
|
Crucible Steel CSM® 6 Tool Steel, AISI A6 CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 427 °C |
6.60 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.60 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 21.1 - 204 °C |
6.60 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |