Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature 500 °C |
6.11 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
Across Surface; ASTM D-696 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature >=100 °C |
6.11 µin/in-°F @Temperature >=212 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 204 °C |
6.11 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 204 °C |
6.11 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
Austenitic |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 425 °C |
6.11 µin/in-°F @Temperature 68.0 - 797 °F |
|
Crucible Steel CPM® REX® 66 (HS) High Speed Steel CPM Rex 66 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed with a high vanadium content for excellent abrasion resistance, simila.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 100 °C |
6.11 µin/in-°F @Temperature 69.8 - 212 °F |
Mean |
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 25.0 - 538 °C |
6.11 µin/in-°F @Temperature 77.0 - 1000 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.11 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 °C |
6.11 µin/in-°F @Temperature 212 °F |
|
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORA.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.11 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |