Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 - 200 °C |
6.67 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 38.0 - 200 °C |
6.67 µin/in-°F @Temperature 100 - 392 °F |
|
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 0.000 - 500 °C |
6.67 µin/in-°F @Temperature 32.0 - 932 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 200 °C |
6.67 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 24.0 - 204 °C |
6.67 µin/in-°F @Temperature 75.2 - 399 °F |
|
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 21.0 - 427 °C |
6.67 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe CBS-50™ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case .. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 37.8 - 538 °C |
6.64 µin/in-°F @Temperature 100 - 1000 °F |
|
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 22.0 - 482 °C |
6.67 µin/in-°F @Temperature 71.6 - 900 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.67 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 100 °C |
6.67 µin/in-°F @Temperature 212 °F |
|
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 500 °C |
6.67 µin/in-°F @Temperature 68.0 - 932 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 0.000 - 500 °C |
6.67 µin/in-°F @Temperature 32.0 - 932 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 38.0 - 427 °C |
6.67 µin/in-°F @Temperature 100 - 801 °F |
|
Latrobe LSS™ MGR™ Tool Steel (ASTM A8) TLS MGR tool steel is an air-hardening tool steel that is characterized by a combination of very good toughness, intermediate wear resistance, and excellent dimensional stability in heat treatment. .. |