Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 300 °C |
6.44 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 200 °C |
6.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Latrobe LSSâ„¢ Chipper Knife Tool Steel (ASTM A8 Mod.) TLS Chipper Knife tool steel is an air-hardening, 8% chromium tool steel which exhibits very good wear resistance and toughness. TLS Chipper Knife exhibits wear resistance which is better than that.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 0.000 - 400 °C |
6.44 µin/in-°F @Temperature 32.0 - 752 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 300 °C |
6.44 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 300 °C |
6.44 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 400 °C |
6.44 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 400 °C |
6.44 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 100 °C |
6.44 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 100 °C |
6.44 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 100 °C |
6.44 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 38.0 - 260 °C |
6.44 µin/in-°F @Temperature 100 - 500 °F |
|
Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel LESCALLOY 52100 VAC-ARC is a deep hardening alloy steel used for aircraft bearings and other high stressed parts where good rolling contact fatigue strength is required at operating temperatures bel.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature -30.0 - 70.0 °C |
6.44 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG39 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 600 °C |
6.44 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 200 °C |
6.44 µin/in-°F @Temperature 68.0 - 392 °F |
Hardened and tempered to 60-62 HRC |
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 300 °C |
6.44 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 200 °C |
6.44 µin/in-°F @Temperature 68.0 - 392 °F |
after high temperature tempering |
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 600 °C |
6.44 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 300 °C |
6.44 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 200 °C |
6.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 500 °C |
6.44 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature <=649 °C |
6.44 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature <=649 °C |
6.44 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 410 Martensitic Stainless steel AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 200 °C |
6.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Annealed Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 25.0 - 100 °C |
6.44 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 600 °C |
6.44 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 600 °C |
6.44 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 0.000 - 400 °C |
6.44 µin/in-°F @Temperature 32.0 - 752 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |
|||
CTE, linear | 11.6 µm/m-°C @Temperature 20.0 - 450 °C |
6.44 µin/in-°F @Temperature 68.0 - 842 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |