Material Notes:
Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corrosive reactionsHardening (Heat Treatment): 1020°C- 1050°C; Quenching: Oil or salt bath, 500-550°C; Hardness: 49 HRC QuenchedInformation provided by Schmolz + Bickenbach
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32
<br>@Treatment Temp. 600.0 °C
32
<br>@Treatment Temp. 1112 °F
46
<br>@Treatment Temp. 300 °C
46
<br>@Treatment Temp. 572 °F
46
<br>@Treatment Temp. 400 °C
46
<br>@Treatment Temp. 752 °F
47
<br>@Treatment Temp. 200 °C
47
<br>@Treatment Temp. 392 °F
47
<br>@Treatment Temp. 500 °C
47
<br>@Treatment Temp. 932 °F
49
<br>@Treatment Temp. 100 °C
49
<br>@Treatment Temp. 212 °F
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C
<br>@Temperature 20.0 - 100 °C
5.83 µin/in-°F
<br>@Temperature 68.0 - 212 °F
10.7 µm/m-°C
<br>@Temperature 20.0 - 150 °C
5.94 µin/in-°F
<br>@Temperature 68.0 - 302 °F
10.8 µm/m-°C
<br>@Temperature 20.0 - 200 °C
6.00 µin/in-°F
<br>@Temperature 68.0 - 392 °F
10.9 µm/m-°C
<br>@Temperature 20.0 - 250 °C
6.06 µin/in-°F
<br>@Temperature 68.0 - 482 °F
11.1 µm/m-°C
<br>@Temperature 20.0 - 300 °C
6.17 µin/in-°F
<br>@Temperature 68.0 - 572 °F
11.3 µm/m-°C
<br>@Temperature 20.0 - 350 °C
6.28 µin/in-°F
<br>@Temperature 68.0 - 662 °F
11.5 µm/m-°C
<br>@Temperature 20.0 - 400 °C
6.39 µin/in-°F
<br>@Temperature 68.0 - 752 °F
11.6 µm/m-°C
<br>@Temperature 20.0 - 450 °C
6.44 µin/in-°F
<br>@Temperature 68.0 - 842 °F
11.7 µm/m-°C
<br>@Temperature 20.0 - 500 °C
6.50 µin/in-°F
<br>@Temperature 68.0 - 932 °F
Thermal Conductivity 23.2 W/m-K
<br>@Temperature 500 °C
161 BTU-in/hr-ft²-°F
<br>@Temperature 932 °F
23.5 W/m-K
<br>@Temperature 23.0 °C
163 BTU-in/hr-ft²-°F
<br>@Temperature 73.4 °F
24.1 W/m-K
<br>@Temperature 400 °C
167 BTU-in/hr-ft²-°F
<br>@Temperature 752 °F
24.2 W/m-K
<br>@Temperature 150 °C
168 BTU-in/hr-ft²-°F
<br>@Temperature 302 °F
24.4 W/m-K
<br>@Temperature 300 °C
169 BTU-in/hr-ft²-°F
<br>@Temperature 572 °F
24.4 W/m-K
<br>@Temperature 350 °C
169 BTU-in/hr-ft²-°F
<br>@Temperature 662 °F
Processing Properties Metric English Comments
Annealing Temperature 760 - 800.0 °C
1400 - 1472 °F
Soft; Cooling: Furnace; &lt; 230 HB
Descriptive Properties Value Comments
Corrosion Properties/Weight loss rate 0.2% Hydrochloric Acid
20 g/hm&lt;sup&gt;2&lt;/sup&gt;
5% Acetic Acid
0.1 g/hm&lt;sup&gt;2&lt;/sup&gt;
5% Nitric Acid
1 g/hm&lt;sup&gt;2&lt;/sup&gt;
5% Sulphuric Acid
90 g/hm&lt;sup&gt;2&lt;/sup&gt;
Copyright © lookpolymers.com All Rights Reserved