Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 50.0 - 150 µm/m-°C | 27.8 - 83.3 µin/in-°F | Average value: 110 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 80.0 - 150 µm/m-°C | 44.4 - 83.3 µin/in-°F | Average value: 133 µm/m-°C Grade Count:6 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
CTE, linear, Transverse to Flow | 50.0 - 150 µm/m-°C | 27.8 - 83.3 µin/in-°F | Average value: 110 µm/m-°C Grade Count:9 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
CTE, linear, Transverse to Flow | 80.0 - 150 µm/m-°C | 44.4 - 83.3 µin/in-°F | Average value: 97.0 µm/m-°C Grade Count:12 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear, Transverse to Flow | 56.0 - 150 µm/m-°C @Temperature 50.0 - 250 °C |
31.1 - 83.3 µin/in-°F @Temperature 122 - 482 °F |
Average value: 104 µm/m-°C Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear, Transverse to Flow | 150 - 150 µm/m-°C @Temperature 60.0 - 138 °C |
83.3 - 83.3 µin/in-°F @Temperature 140 - 280 °F |
Average value: 150 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |