Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EXABS01 ABS
Sheet extrusion ABS with medium impact.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® GX3800F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58 ABS
High impact ABS for sheet extrusion and blow molding applications.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -30.0 - 30.0 °C
57.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer
LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -30.0 - 30.0 °C
57.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66
LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 104 µm/m-°C

@Temperature -30.0 - 30.0 °C
57.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer
LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 104 µm/m-°C
57.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 104 µm/m-°C
57.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p..