Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
43.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East) LNP* Thermocomp* IB008 is a compound based on Nylon 6/12 resin containing Glass Bead. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C | 43.9 µin/in-°F | ISO 11359 |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C | 43.9 µin/in-°F | ISO 11359 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature 20.0 °C |
43.9 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |